MDI-prepolymeer
hurdens: shore A 75A - shore A 95A
It produkt hat de skaaimerken fan goede wearzebestriding, fearkrêft en poerbêste meganyske eigenskippen.
Brûkt foar it meitsjen fan ferskate polyurethaan-elastomeerprodukten lykas rubberen tsjillen, sieveplaten en ôfslutingsringen.
|
Model
| D2560 | D2575 | D2590 | D3565 | D3575 | D3590 |
| NCO/% | 6.0±0.2 | 7,5 ± 0,2 | 9.0±0.2 | 6,5 ± 0,2 | 7,5 ± 0,2 | 9.0±0.2 |
| Steat by 20 ℃ | PTMG-systeem, wyt fêst | Polyester systeem, wyt fêst | ||||
| BDO100g Prepolymeer /g | 6.1 | 7.8 | 9.3 | 6.8 | 7.8 | 9.3 |
| Viskositeit (85℃)/mPa·s | 1400 | 1000 | 750 | 1400 | 1200 | 1000 |
| Mingtemperatuer /℃ (Prepolymeer /1,4BD) | 80/40 | 80/40 | 80/40 | 80/40 | 80/40 | 80/40 |
| Geltiid /min | 10 | 8 | 7 | 10 | 8 | 7 |
| Nei-vulkanisaasjetiid (110 ℃)/oere | 48 | 48 | 48 | 48 | 48 | 48 |
| Hurdens (Shore A) | 87±2 | 90±2 | 95±2 | 85±2 | 90±2 | 95±2 |
| 100% Modulus/MPa | 6 | 9.2 | 12.6 | 5 | 8.6 | 12.3 |
| 300% Modulus / MPa | 17 | 16.6 | 18.9 | 10 | 19.7 | 29.1 |
| Treksterkte / MPa | 44 | 43 | 45 | 50 | 46 | 55 |
| Ferlinging / % | 472 | 683 | 500 | 540 | 580 | 530 |
| Skuorreftichheid / (KN/m²) | 75 | 110 | 130 | 82 | 117 | 132 |
| Rebound / % | 61 | 64 | 55 | 43 | 35 | 39 |
| Dichtheid (24 ℃) / (g/ cm3) | 1.11 | 1.11 | 1.12 | 1.23 | 1.26 | 1.24 |
| Din wear /mm³ | 36 | 44 | 44 | 32 | 35 | 38 |