Donfoam 823PIR CP/IP mixtura polyolorum basis ad spumam PIR continuam formandam
Donfoam 824PIR HFC-245fa mixtura basis polyolorum pro spuma PIR continua
INTRODUCTIO
Donfoam823 mixtura polyetheris polyoli CP vel CP/IP ut agens inflans adhibetur, in productione spumae PIR ignifugae altae, cum effectu cellulae spumae uniformis, conductivitatis thermalis humilis, bonae insulationis thermalis et ignifugae altae, temperaturae humilis nullae fissurae contrahentis etc. Late adhibetur in processu omnium generum operis insulationis, ut: aedificatio muri externi, repositio frigida, cisternae, tubi magni etc.
PROPRIETAS PHYSICA
| Aspectus Viscositas dynamica (25℃) mPa.S Densitas (20℃) g/ml Temperatura repositionis ℃ Mensis stabilitatis repositionis | Liquor pellucidus pallide flavus vel fuscus 500±100 1.20±0.1 10-25 6 |
PROPORTIO COMMENDATA
| Res | PBW |
| DK-1103 Mixtura Polyetheris Polyoli CP vel CP/IP Isocyanas | centum XI-XIII 165-175 |
TECHNOLOGIA ET REACTIVITAS(valor exactus variat secundum condiciones processus)
| Mixtio Manualis | |
| Temperatura Materiae Crudae ℃ Temperatura mucoris ℃ CT GT TFT Densitas Libera kg/m²3 | XX-XXV Temperatura ambientis (15-45℃) XXXV-LX 140-200 240-360 XXVIII-XXXV |
SPUMAE PERFORMANTIAE
| Res | Norma Probationis | Specificatio |
| Densitas Totalis Formationis Densitas Nuclei Formandi | ASTM D1622 | ≥50kg/m²3 ≥40kg/m² |
| Frequentia Cellae Clausae | ASTM D2856 | ≥90% |
| Conductivitas Thermalis Initialis (15℃) | ASTM C518 | ≤24mW/(mK) |
| Robur Compressivum | ASTM D1621 | ≥150kPa |
| Stabilitas Dimensionalis 24h -20℃ RH90 70℃ | ASTM D2126 | ≤1% ≤1.5% |
| Ratio Absorptionis Aquae | ASTM D2842 | ≤3% |
| Inflammabilitas | ASTM D1692 | Sui extinguibilis |