I-Donpanel 415 / PIR iyindawo equkethe ama-polyols, ama-surfactants, ama-catalysts, ne-flame retardant, ingxube ye-HFC-245FA njenge-ejenti evuthayo ngesilinganiso esikhethekile. I-Foam inendawo enhle yokufakelwa okushisayo, isisindo esikhanyayo, amandla aphezulu okucindezela kanye ne-flame retardant nezinye izinzuzo. Kusetshenziswa kabanzi ukukhiqiza amapuleti we-sandwich, amaphaneli ahlanganisiwe njll, okusebenza ukwenza izitolo ezibandayo, amakhabethe, izindawo zokukhosela eziphathwayo njll.
Impahla yenyama
| Donpanel 415 / PIR | Isethulo | |
| Ukubonakala | Ophuzi ophuzi ku-brown ketshezi | Uketshezi olunsundu |
| I-Hydroxyl value mgkoh / g | 200-300 | N / a |
| I-Viscosity Enamandla (25 ℃) MPA.S | 300-500 | 200-250 |
| Amandla athile adonsela phansi (20 ℃) g / ml | 1.10-1.16 | 1.20-1.25 |
| Ukushisa okushisa ℃ | 10-25 | 10-25 |
| Isitoreji inyanga yokuqina | 6 | 12 |
Isilinganiso esinconyiwe
| Ama-Raw material | Uhlobo |
| Donpanel 415 / PIR | 100 |
| Isocyanate | 130-150 |
Ubuchwepheshe nokuvuselelwa kabusha(Inani eliqondile liyahlukahluka ngokuya ngezimo zokucubungula)
| Into | Ukuxuba okwenziwa ngesandla | Umshini wokuhlobisa wengcindezelo ephezulu |
| Izinga lokushisa elibonakalayo ℃ | 20-25 | 20-25 |
| Ukushisa kokubumba ℃ | 35-45 | 35-45 |
| Isikhathi sekhilimu | 30-50 | 20-30 |
| Isikhathi se-gel | 120-200 | 70-150 |
| MAHHALA KG / M3 | 28-31 | 27-30 |
Ukusebenza kwe-Foam
| Ubuningi bokubumba | I-ASTM D 1622-08 | ≥45kg / m3 |
| Okuqukethwe kweseli okuvaliwe | I-ASTM D 2856 | ≥90% |
| I-Thermal Creativity (23 ℃) | I-ASTM C 518-10 | ≤24mw / (mk) |
| Amandla okucindezela | I-ASTM D 1621-10 | ≥140kpa |
| Ukuqina okungama-24h -20 ℃ 24h 100 ℃ | I-ASTM D 2126-09 | ≤1% ≤1.5% |
| Ukuvulayo | I-DIN4102 | B2 |
Imininingwane enikezwe ngenhla iyinani elijwayelekile, elihlolwe yinkampani yethu. Ngemikhiqizo yenkampani yethu, imininingwane efakiwe emthethweni ayinazo izingqinamba.